产品规格

项目

指标

Al2O3 %

≤3

SiO2 / %

≥95

CaO / %

≤3

残余石英 / %

≤10

体积密度 (kg/m3)

as received

≥1800

after 1300℃ / 5 hours

≥1850

真密度 /(kg/m3)

as received

≤2100

after 1300℃ / 5 hours

≤2350

显气孔率 / %

as received

Avg. <18

after 1300℃ / 5 hours

Avg. <20

常温耐压强度 / MPa(N/mm2)

as received

≥30

热膨胀率 / %

growth at 1300℃

≥0

between 0 and 300 hours

≤0.2

蠕变率

1500℃ / 20-50 N/mm2

≤0.2

导热系数 1100℃ W/m.k

250℃

≥1.1

1000℃

≥2.0